电极糊是供给铁合金炉,电石炉作消耗性导电材料的自焙电极,通过电流产生热量使之焙烧成为导电电极用于冶炼
Electrode paste is used as consumptive conductive material------self-roasting electrode in the iron-alloy furnace and the ecetylene furnace.Electrode paste brings obout caloric in the furnace byelectric current,the caloric makes electrode paste baked to be conductive electrode for smelting.
规格和指标:
Specifications and properties:
1).1号糊(THD-1):
灰分(Ash)5.0%以下,
挥发份(V.M.)12.0%-15.5%,
抗压强度1(Compressive Strength)7.0Mpa以上,
电阻率(Resistivity)68μΩm以下,
体积密度(Bulk Density)1.36G/CM3以上。
2).2号糊(THD-2,):
灰分(Ash )6.0%以下,
挥发份(V.M.)12.0%-15.5%,
抗压强度(Compressive Strength )15.7Mpa以上,
电阻率(Resistivity)75μΩm以下,
体积密度(Bulk Density )1.36G/CM3以上。
3).3号糊(THD-3):
灰分(Ash)7.0%以下,
挥发份(V.M.)9.5%-13.5%,
抗压强度( Compressive Strength )19.6Mpa以上,
电阻率(Resistivity)80μΩm以下,
体积密度(Bulk Density )1.36G/CM3以上。
4).4号糊(THD-4):
灰分(Ash)9.0%以下,
挥发份(V.M.)11.5%-15.5%,
抗压强度( Compressive Strength )19.6Mpa以上,
电阻率(Resistivity)90μΩm以下,
体积密度(Bulk Density )1.36G/CM3以上。
5).5号糊(THD-5,):
灰分(Ash)11.0%以下,
挥发份(V.M.)11.5%-15.5%,
抗压强度(Compressive Strength )19.6Mpa以上,
电阻率(Resistivity)90μΩm以下,
体积密度(Bulk Density )1.36G/CM3以上。
固定碳 | .(%) | 规格 | THD1(目) |
牌号 | HJ | 水分 | -(%) |
膨胀度 | -(倍) | 筛上物粒度 | -(%) |
灰分 | 5.0% | 挥发分 | 12.0-15.5(%) |
筛下物粒度 | -(%) |